Data Sheet

926

UNS N08926
Bars
Sheets/Plates
Material

926 Steel

International Codes

UNS N08926

NiCrMoCuN25-20-7

14,529

Main Features

Corrosion Resistant

Density

8,1Kg/dm3

Chemical Composition

Cr

20-21%

Ni

24-26%

Mo

6-7%

Co

NbTa

Al

Ti

C

Max. 0,02%

Fe

Mn

Max. 1%

Si

Max. 0,5%

P

Max. 0,010%

S

Max. 0,010%

CbTa

Cu

0,5-1,5%

Altro

Standards

ASTM

A240, B625, B649

API

5LD

NACE

MR0175

General Proprieties

The austenitic stainless steel 926 (UNS N08926) was developed on basis of 904L steel. However, the molybdenum content at 926 steel was raised to 6.5%. The 926 steel has excellent general corrosion resistance and improved resistance to pitting and crevice corrosion. The resistance to stress corrosion cracking is also increased. It is often referred as super austenitic stainless steel. The 926 steel is available at CHUN & VOLLERIN in the following formats: Bars, Plates.
All data are to be considered typical for the product selected. Refer to the production certificate for the specific characteristics of the product. All the material has a UNI EN 10240 3.1 certificate with EU, USA and JP origin. All registered trademarks are the property of their respective owners.

Ask quotation

Please fill the form or send your request via email

write us by email

926

Il seguente campo NON deve essere compilato.